Pure zirconia is monoclinic at room temperature, tetragonal at high temperature and cubic near its melting point. Adding about 3 mole percent of yttria holds the tetragonal phase in a metastable state at room temperature. When a crack begins to run, the tensile stress at its tip triggers the tetragonal grains there to transform into the monoclinic form, which occupies three to five percent more volume; the expansion puts the region around the crack into compression and arrests it. This transformation toughening gives yttria-stabilised zirconia the highest flexural strength and fracture toughness of the dental ceramics, suiting it to posterior frameworks, monolithic crowns and bridges and implant abutments. Because it is fully polycrystalline with no glass phase it cannot be etched with hydrofluoric acid, and bonding relies on alumina air abrasion and a phosphate monomer primer; it is also susceptible to slow low-temperature degradation in moisture. Option A has the lowest strength and is used for veneering. Option B gains strength from an interlocking network of needle-like crystals, is etchable and highly aesthetic. Option D is strengthened by dispersed leucite crystals that deflect cracks, but far less. Exam tip: no glass means no etching, so zirconia is primed, not etched.